YM10 LAO (001) at 1000C_Sr closed_SnO2 closed.img 615070 2018-05-24T04:58:17Z
YM10 LAO (001) at 1150C_Sr closed_SnO2 closed after 15 min degasing.img 615070 2018-05-24T05:17:52Z
YM10 LAO (001) at 280C_Sr 510C_SnO2 closed_gate valved opend then closed.img 615040 2018-05-24T14:38:11Z
YM10 LAO (001) at 280C_Sr closed_SnO2 closed before Sr deposition.img 615070 2018-05-24T05:37:34Z
YM10 LAO (001) at 350C_Sr closed_SnO2 closed.img 615070 2018-05-24T04:37:34Z
YM10 LAO (001) at 500C_Sr closed_SnO2 closed.img 615070 2018-05-24T04:44:30Z
YM10 LAO (001) at 600C_Sr closed_SnO2 closed.img 615070 2018-05-24T04:50:36Z
YM10 LAO (001) at 831C_Sr closed_SnO2 closed.img 615070 2018-05-24T04:55:08Z